Flash rust needs three things: iron, oxygen and water. A wet steel part sitting in open air has all three, so those conditions are always present. The work is finding what tips them over.
1. Parts drying mid-process. This is the big one. A part that dries before it reaches conversion coating leaves bare steel in open air. Slow line speeds and line stoppages are where it happens most.
2. High washer temperatures. Hotter stages evaporate water faster, which gets the part to a dry, exposed surface sooner.
3. Water impurities. Dissolved salts and minerals in rinse water act as accelerators.
4. Acidic pH. Low pH in the cleaner or rinse baths drives rust formation aggressively.
5. Uneven chemical coverage. Clogged nozzles or weak tank agitation leave dry shadows where the part isn’t protected.
Start with the timing question. If parts are drying between stages, fix that before looking at chemistry. Then work through the water, the pH and the spray pattern.